Cobalt-chromium-tungsten Alloy

  • form:sheet ,coil ,strip ,bar ,tube,wire
  • Supply capacity: more than 5000T
  • From the quantitative: more than 1T
  • Delivery time: 3-45 days
  • Port Delivery:Shanghai
Share to

Introduction

 CoCrWalloy is a range of cobaltchromium alloys designed for wear resistance. 

It is a completely nonmagnetic and corrosionresistant cobalt alloy. 

There are a number of Stellite alloys, with various compositions 

optimised for different uses. Some are formulated to maximize combinations of wear resistance, corrosion resistance, or ability to withstand extreme temperatures

 

Features:

1. Heat Resistance, wear resistance, corrosion resistance

 2. Made as required dimensions and materials

 3. Main products: valve seat, pump parts, pistons, bushings, nozzles etc

 

 Compositions:

Brand and No Carbon(Min-Max) Manganese(Min-Max) Sillicon(Min-Max) Chrom(Min-Max) Nickel Moly Tung Cobalt(Min-Max) Iron Other
     
(Min-Max) (Min-Max) (Min-Max)
CoCrW3 2.00-2.70 1 1 29.0-33.0 3   11.0-14.0 Bal. 3 P.03MAX
 
S.03MAX
CoCrW4 1 1 1.5 28.0-32.0 3 1.5 12.5-15.5 Bal. 3  
CoCrW6 .90-1.4 1 1.5 27.0-31.0 3 1.5 3.50-5.50 Bal. 3 P.04MAX
 
S.04MAX

 

Physical Properties:

Item. CoCrw3 CoCrW6 CoCrW12 CoCrW394 TTG25 TTG25 Blade
 
(CFB)
Hardness 51-55 38-44 44-49 47-51 57-60 60-63 46.5-50

 

Stellit 6 Physical property (Room Temp.)

Density Specific Solidus Liquidus Specific heat Magnetic Electrode Electrical Electrical
(lb/in³) Gravity (J/kg·K) Permeability Potential Conductivity Resistivity
0.305 8.46 2340°F 2540°F 0.101°F <1.2@200 -0.25 1.9%IACS 41.73
Btu/lb- Oersteds Volts (Int. Annealed Copper Std.) microhms-inch

 

 Stellite 6 Thermal Properties-Conductivity & Expansion

Thermal Expansion Coefficient Thermal Conductivity by Temperature
°F Microinch/ °C Microns/ °F Btu/ft2/in/ °C W/mk
inch-°F m-°C hr/°F
212 6.3 100 11.34 70 102.7 21.11 14.82

 